本文选取使用前和重复使用不同次数后的某动力装置输运管道壳体材料进行金相分析、晶粒度和力学性能等测试,确定金属壳体使用前及重复使用不同次数后材料性能的变化规律,验证衰变规律,评估输运管道金属壳体重复使用能力。实验结果表明,重复使用1次后,输运管道材料12Cr1MoVG的冲击韧性和断裂韧性可能降低到临界值以下,某动力装置的安全性和可靠性将受到影响。
In this paper, the material of elbow shell pre-use and after repeated use for different times was selected for metallographic analysis; grain fineness number and mechanical properties etc. test. The verification of the decay laws, determining the law of changes in material properties before and after different times of use of metal shell, Assess the reusability of the propulsion system's metal shell. The experimental results show that, after one time repeated use the impact toughness and fracture toughness of the elbow shell material 12Cr1MoVG may be reduced below the critical value. The safety and reliability of the propulsion system will be affected.
2021,43(11): 179-184 收稿日期:2021-06-03
DOI:10.3404/j.issn.1672-7649.2021.11.034
分类号:TJ04
作者简介:汪太琨(1966-),女,研究员,主要从事导弹发射技术研究
参考文献:
[1] 赵险峰, 等. 潜地弹道导弹发射系统内弹道学[M]. 哈尔滨: 哈尔滨工程大学出版社, 2000.
[2] 赵世平. 潜地弹道导弹变深度发射某动力装置有用能调节机理研究[D]. 西安: 西北工业大学, 2006.
[3] 黄道远. 热/力作用下钴基硬质合金组织性能变化及相关机理的研究[D]. 长沙: 中南大学, 2010.
[4] 刘爱辉. 12Cr1MoV钢动态断裂韧度的研究[D]. 哈尔滨: 哈尔滨理工大学, 2004.
[5] 全国钢标准化技术委员会. 金属显微组织检验方法:GB/T 13298-2015[S]. 北京:中国标准出版社, [2015-09-11].
[6] 全国钢标准化技术委员会. 钢中非金属夹杂物含量的测定标准评级图显微检验法:GB/T 10561-2005[S]. 北京:中国标准出版社, [2005-05-13].
[7] 全国钢标准化技术委员会. 金属平均晶粒度测定方法: GB/T 6394-2017[S]. 北京:中国标准出版社, [2017-11-01].
[8] 全国钢标准化技术委员会. 钢的脱碳层深度测定方法: GB/T 224-2008[S]. 北京:中国标准出版社, [2008-08-05].
[9] 全国钢标准化技术委员会. 钢材 夏比V型缺口摆锤冲击试验仪器化试验方法: GB/T 19748-2005[S]. 北京:中国标准出版社, [2005-05-13].
[10] 全国钢标准化技术委员会. 金属材料 准静态断裂韧度的统一试验方法: GB/T 21143-2014[S]. 北京:中国标准出版社, [2014-12-15].